TDS PDF

↑
St AS 4133.3.4-2005 (2016)

Methods of testing rocks for engineering purposes, Method 3.4: Rock swelling and slake durability tests — Determination of the slake durability index of rock samples. Original standard AS 4133.3.4-2005 (2016) in PDF full version. Additional info + preview on request

Document status: Active

€35
St AS 4133.4.1-2007 (2016)

Methods of testing rocks for engineering purposes, Method 4.1: Rock strength tests — Determination of point load strength index. Original standard AS 4133.4.1-2007 (2016) in PDF full version. Additional info + preview on request

Document status: Active

€35
St AS 4133.4.2-1993

Methods of testing rocks for engineering purposes, Method 4.2: Rock strength tests — Determination of uniaxial compressive strength. Original standard AS 4133.4.2-1993 in PDF full version. Additional info + preview on request

Document status: Replaced by

€35
St AS 4133.4.2.1-2007

Methods of testing rocks for engineering purposes, Method 4.2.1: Rock strength tests — Determination of uniaxial compressive strength of 50 MPa and greater. Original standard AS 4133.4.2.1-2007 in PDF full version. Additional info + preview on request

Document status: Replaced by St AS 4133.4.2.1-2022

€35
St AS 4133.4.2.1-2022

Methods of testing rocks for engineering purposes, Method 4.2.1: Rock strength tests — Determination of uniaxial compressive strength — Rock strength greater than 50 MPa. Original standard AS 4133.4.2.1-2022 in PDF full version. Additional info + preview on request

Document status: Active

€35
St AS 4133.4.2.2-2013

Methods of testing rocks for engineering purposes, Method 4.2.2: Rock strength tests — Determination of uniaxial compressive strength — Rock strength less than 50 MPa. Original standard AS 4133.4.2.2-2013 in PDF full version. Additional info + preview on request

Document status: Active

€35
↑