TDS PDF
Steel, Heat-Resistant, Bars, Forgings, and Tubing 0.95Cr - 0.55Mo - 0.30V (0.40 - 0.50C) Vacuum Arc Remelted. Original standard SAE AMS 6305G-2016 in PDF full version. Additional info + preview on request
Document status: Replaced by St SAE AMS6305H-2023
Steel, Bars and Forgings 0.90Si - 1.0Cr - 2.0Ni - 3.2Mo - 2.0Cu - 0.10V (0.07 - 0.13C) Vacuum Arc or Electroslag Remelted. Original standard SAE AMS 6308F-2018 in PDF full version. Additional info + preview on request
Document status: Replaced by St SAE AMS6308G-2023
Steel Bars, Forgings, and Tubing 1.8Ni - 0.25Mo (0.38 - 0.43C) (4640). Original standard SAE AMS 6312J-2015 in PDF full version. Additional info + preview on request
Document status: Replaced by St SAE AMS6312L-2025
Steel Bars and Forgings 1.8Ni - 0.25Mo (0.38 - 0.43C) (4640) Heat Treated, 125 ksi (862 MPa) Tensile Strength. Original standard SAE AMS 6317K-2017 in PDF full version. Additional info + preview on request
Document status: Replaced by St SAE AMS6317L-2022
Steel Bars, Forgings, and Rings 0.50Cr - 0.55Ni - 0.25Mo (0.33 - 0.38C) (8735). Original standard SAE AMS 6320P-2017 in PDF full version. Additional info + preview on request
Document status: Replaced by St SAE AMS6320R-2023
Steel Bars, Forgings, and Rings 0.50Cr - 0.55Ni - 0.25Mo (0.38 - 0.43C) (SAE 8740). Original standard SAE AMS 6322P-2014 in PDF full version. Additional info + preview on request
Document status: Replaced by St SAE AMS6322S-2023